Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | Lubrizol Advanced Materials, Inc. |
Trademark: | Estane® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | y9MylF_Estane-58300-TPU.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Type: Polyether Thermoplastic Polyurethane (TPU) Special Feature: Moisture Vapor Transmission, with Excellent Hydrolysis Resistance, Low Temperature and Wide Process Window Processes: Extrusion: Blown, Flat Die Cast Film, Injection and Cable Jacketing |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.10 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 82 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Taber Abrasion Resistance (1000 Cycles, 1000 g, H-18 Wheel) | 22.0 | mg | ASTM D3389 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Water Vapor Transmission | 450 | g/m²/24 hr | ASTM E96 |
Water Vapor Transmission - Mocon 1(38°C, 25.4 µm) | 1800 | g/m²/24 hr | ASTM D6701 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Kofler Melting Temperature | 125 | °C | Internal method |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set (200% Strain) | 11 | % | ASTM D412 |
Tensile Stress | ASTM D412 | ||
100% strain, 0.762mm | 4.80 | MPa | ASTM D412 |
300% strain, 0.762mm | 7.60 | MPa | ASTM D412 |
Tensile Strength (Break, 0.762 mm) | 37.9 | MPa | ASTM D412 |
Tensile Elongation (Break, 0.762 mm) | 650 | % | ASTM D412 |
Tear Strength | |||
0.762 mm 2 | 69.6 | kN/m | ASTM D624 |
Cracking | 23 | kN/m | ASTM D470 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -50.0 | °C | ASTM D3418 |
Melting Temperature | 130 | °C | DSC |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 104 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Suggested Max Moisture | 0.020 | % | |
Cylinder Zone 1 Temp. | 166 | °C | |
Cylinder Zone 2 Temp. | 171 | °C | |
Cylinder Zone 3 Temp. | 177 | °C | |
Cylinder Zone 4 Temp. | 182 | °C | |
Adapter Temperature | 182 | °C | |
Melt Temperature | 179 | °C | |
Die Temperature | 182 | °C |
Extrusion instructions |
---|
Screens: 20-40-80 meshDew Point: -40°C |
Note Message | |
---|---|
1 . | 90% RH |
2 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 805 SI 2 | RTP Company | Acetal (POM) Copolymer | RTP |
Resinoid 2020 | Resinoid Engineering Corporation | Phenolic | Resinoid |
ACCULOY™ POL062L | ACLO Compounders Inc. | PC+PET | ACCULOY™ |
Glastic® 2450-15 | Glastic Corporation | Polyester, TS | Glastic® |
Pro-fax SB912 | LyondellBasell Industries | PP Copolymer | Pro-fax |