Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | w2VfSm_SarlinkTPEFM2270XRD1PRELIMINARYDATA.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Sarlink FM-2270 XRD1 is a general purpose thermoplastic elastomer, available in NAT, BLK, and colors, designed for automotive interior applications, including floor mats. Sarlink FM-2270 XRD1 is a UV stabilized, medium hardness, high density, wear-resistant, filled grade with good wear resistance and suitable for injection molding. |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.18 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 12 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ISO 868 | ||
Shore A, 1 second, injection molding | 73 | ISO 868 | |
Shore A, 5 seconds, injection molding | 71 | ISO 868 | |
Shore A, 15 seconds, injection molding | 70 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 1.80 | MPa | ISO 37 |
Tensile Stress (Break) | 5.00 | MPa | ISO 37 |
Tensile Elongation (Break) | 700 | % | ISO 37 |
Tear Strength | 24 | kN/m | ISO 34-1 |
Legal statement |
---|
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 199 - 210 | °C | |
Middle Temperature | 204 - 216 | °C | |
Front Temperature | 210 - 221 | °C | |
Nozzle Temperature | 216 - 227 | °C | |
Processing (Melt) Temp | 216 - 227 | °C | |
Mold Temperature | 35 - 66 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 120 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 205 D FR | RTP Company | Nylon 612 | RTP |
RTP 800 DEL | RTP Company | Acetal (POM) Homopolymer | RTP |
ADDILENE J 220 M20 | ADDIPLAST | PP Copolymer | ADDILENE |
Flontech® FT-BRR40-2 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
KOCETAL® GF304 | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |