Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
Manufacturer: | Techmer Engineered Solutions |
Trademark: | Plaslube® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | rCGgxP_Plaslube-AC-80-TF-2.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Plaslube®AC-80/TF/2 is a polyoxymethylene (POM) copolymer product,. It can be processed by injection molding and is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. Typical application areas are: engineering/industrial accessories. Features include:
|
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.41 | g/cm³ | ASTM D792 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break, 23°C) | 58.6 | MPa | ASTM D638 |
Flexural Modulus (23°C) | 2410 | MPa | ASTM D790 |
Flexural Strength (Break, 23°C) | 82.7 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 37 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 118 | °C | ASTM D648 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 82.2 | °C | |
Drying Time | 1.0 - 2.0 | hr | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 177 - 188 | °C | |
Middle Temperature | 188 - 199 | °C | |
Front Temperature | 182 - 193 | °C | |
Nozzle Temperature | 177 - 188 | °C | |
Processing (Melt) Temp | 188 - 204 | °C | |
Mold Temperature | 76.7 - 93.3 | °C | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.345 - 0.689 | MPa |
Injection instructions |
---|
Screw Speed: MediumRecommendations for Molding and Tool Conditions: Well ventedMoisture Content, as received: Product is packaged at 0.2% or less.Drying not normally required. Dry at 180°F for 1 to 2 hours if necessary. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 300 AR 10 | RTP Company | PC | RTP |
Ultramid® A3W2G10 BK20560 | BASF Corporation | Nylon 66 | Ultramid® |
Xuchuan 3070/B-8280 | Xuchuan Chemical (Suzhou) Co., Ltd | TPU-Polyester | Xuchuan |
ETILINAS BPD 3220 | POLYETHYLENE MALAYSIA SDN BHD | LLDPE | ETILINAS |
3M™ Dyneon™ Fluoroelastomer FE 5830Z | 3M Advanced Materials Division | Fluorelastomer | 3M™ Dyneon™ Fluoroelastomer |