Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Asia International Enterprise (Hong Kong) Limited |
Trademark: | AIE PP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | qISgv4_AIE-PP-80G4.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
AIE PP 80G4 is a polypropylene material, which contains a 20% glass fiber reinforced material. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is injection molding. The main features of AIE PP 80G4 are:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.03 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 8.0 | g/10 min | ISO 1133 |
Molding Shrinkage | 0.20 - 0.50 | % | Internal method |
Water Absorption (23°C, 24 hr) | 0.10 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 90.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 6.0 | % | ISO 527-2 |
Flexural Modulus | 4400 | MPa | ISO 178 |
Flexural Stress | 140 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 4.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, not annealed | 155 | °C | ISO 75-2/B |
1.8 MPa, not annealed | 125 | °C | ISO 75-2/A |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 120 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Rear Temperature | 200 - 230 | °C | |
Middle Temperature | 210 - 230 | °C | |
Front Temperature | 210 - 230 | °C | |
Nozzle Temperature | 200 - 220 | °C | |
Mold Temperature | 40.0 - 60.0 | °C | |
Injection Pressure | 30.0 - 120 | MPa | |
Holding Pressure | 40.0 - 50.0 | MPa | |
Back Pressure | 5.00 - 10.0 | MPa | |
Screw Speed | 40 - 60 | rpm |
Injection instructions |
---|
Cylinder Temperature 4: 180 to 200°C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Tecolen® HP30 KG30 NL HS 0B | Eurotec Engineering Plastics | PP Homopolymer | Tecolen® |
Chemlon® MDF4L | Teknor Apex Company (Chem Polymer) | Nylon 6 | Chemlon® |
Delrin® 311DP NC010 | DuPont Performance Polymers | Acetal (POM) Homopolymer | Delrin® |
ELASTOSIL® M 4500 | Wacker Chemie AG | Silicone | ELASTOSIL® M |
Luranyl® HT 240 G4 | ROMIRA GmbH | PPE+Nylon 66 | Luranyl® |