| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | RJM International, Inc. |
| Trademark: | RJM |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 1dyAGA_RJM-SN502-NH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| RJM SN502-NH is a Polyamide 6 (Nylon 6) product. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Typical application: Additive/Masterbatch. Primary characteristic: flame rated. |
| General Information | |
|---|---|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.22 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow | 1.2 to 1.6 | % | ASTM D955 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 60.8 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 10 | % | ASTM D638 |
| Flexural Modulus | 2650 | MPa | ASTM D790 |
| Flexural Strength | 76.5 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | 59 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | 70 | °C | ASTM D648 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | V-0 | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 120 | °C | |
| Drying Time | 3.0 | hr | |
| Processing (Melt) Temp | 230 to 250 | °C | |
| Mold Temperature | 60.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Tarnamid® T- 27 MCS I | Grupa Azoty S.A. | Nylon 6 | Tarnamid® |
| Vydyne® R550 | Ascend Performance Materials Operations LLC | Nylon 66 | Vydyne® |
| Adell PP EA-14 | Adell Plastics, Inc. | PP Homopolymer | Adell PP |
| Geon™ Vinyl Rigid Extrusion L4794 | PolyOne Corporation | PVC, Rigid | Geon™ Vinyl Rigid Extrusion |
| OP - PC - Filled PC 20CCF | Oxford Polymers | PC | OP - PC - Filled |