POLYfill PP EIP5025 F

Category: PP+EPDM , Polypropylene + EPDM Rubber
Manufacturer: Polykemi AB
Trademark: POLYfill
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: qAuZVZ_POLYfill-PP-EIP5025-F.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Mineral reinforced PP Modified, Heat resistant
General Information
Filler / Reinforcement
  • Mineral, 25% Filler by Weight
Features
  • High Heat Resistance
PhysicalNominal ValueUnitTest Method
Density 1.08g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)5.0g/10 minISO 1133
Molding Shrinkage ISO 294-4
    Across Flow 0.90 to 1.1%
    Flow 0.90 to 1.1%
MechanicalNominal ValueUnitTest Method
Tensile Stress 22.0MPaISO 527-2
Tensile Strain (Yield)6.0%ISO 527-2
Flexural Modulus (23°C)1900MPaISO 178
Flexural Stress 40.0MPaISO 178
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength ISO 179
    -40°C 2.5kJ/m²
    -30°C 3.5kJ/m²
    -20°C 5.0kJ/m²
    23°C 15kJ/m²
Charpy Unnotched Impact Strength ISO 179
    -40°C No Break
    -30°C No Break
    -20°C No Break
    23°C No Break
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature 1
    0.45 MPa, Unannealed 125°CISO 75-2/B
    1.8 MPa, Unannealed 70.0°CISO 75-2/A
Vicat Softening Temperature
    -- 149°CISO 306/A50
    -- 73.0°CISO 306/B50
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.60 mm)HBUL 94
Glow Wire Ignition Temperature (2.00 mm)750°CIEC 60695-2-13
Note Message
1 .120°C/hr
Resin Grade Manufacturer Category Trademark
Ultramid® HFX 32 BASF Corporation Nylon 6 Ultramid®
Kepital® F10-03H M KEP Americas Acetal (POM) Copolymer Kepital®
Karina COMP. PVC IVORY 856-35/ 1-DY-IS-LMP Karina Ind. e Com. de Plásticos Ltda PVC, Unspecified Karina
Braskem PP DR152.02 Braskem Europe GmbH PP Random Copolymer Braskem PP
Sylvin 9925-85 BLACK Sylvin Technologies Incorporated PVC, Unspecified Sylvin