| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.12 | -- | g/cm³ | ISO 1183 |
| Water Absorption | ISO 62 | |||
| Saturation, 23°C | 8.0 | -- | % | |
| Equilibrium, 23°C, 50% RH | 2.5 | -- | % |
| Hardness | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Ball Indentation Hardness | 55.0 | 30.0 | MPa | ISO 2039-1 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 1300 | 500 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 40.0 | 30.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield) | 35 | 40 | % | ISO 527-2 |
| Nominal Tensile Strain at Break | > 50 | > 50 | % | ISO 527-2 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | |||
| -30°C | 3.0 | 3.0 | kJ/m² | |
| 23°C | 15 kJ/m² | No Break | ||
| Charpy Unnotched Impact Strength | ISO 179/1eU | |||
| -30°C | No Break | No Break | ||
| 23°C | No Break | No Break |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, Unannealed | 110 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 45.0 | -- | °C | ISO 75-2/A |
| Continuous Use Temperature | Internal Method | |||
| -- 1 | 70.0 to 90.0 | -- | °C | |
| -- 2 | 160 | -- | °C | |
| Melting Temperature 3 | 220 | -- | °C | ISO 11357-3 |
| CLTE | ISO 11359-2 | |||
| Flow | 1.1E-4 | -- | cm/cm/°C | |
| Transverse | 1.6E-4 | -- | cm/cm/°C |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface Resistivity | -- | 1.0E+10 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+13 | 1.0E+12 | ohms·cm | IEC 60093 |
| Electric Strength | 26 | 22 | kV/mm | IEC 60243-1 |
| Comparative Tracking Index | -- | 450 | V | IEC 60112 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Flammability Classification (0.800 mm) | HB | -- | IEC 60695-11-10, -20 |
| Additional Information | Dry | Conditioned | Test Method | |
|---|---|---|---|---|
| ISO Type | PA6-P, E, 24-010 | -- | ISO 1874 |
| Note Message | |
|---|---|
| 1 . | Long Term |
| 2 . | Short Term |
| 3 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Medalist® MD-50253 | Teknor Apex Company | TPE | Medalist® |
| NYCOA Polyamide 851 | Nycoa (Nylon Corporation of America) | Nylon 6 | NYCOA Polyamide |
| ASI POLYPROPYLENE 1579 | A. Schulman Inc. | PP Impact Copolymer | ASI POLYPROPYLENE |
| LAPEROS® A150 | Polyplastics Co., Ltd. | LCP | LAPEROS® |
| Ultrathene® UE650028 | LyondellBasell Industries | EVA | Ultrathene® |