The Sarlink ME-2300 Series is a high performance thermoplastic elastomer series, available in BLK, designed for automotive exterior molded applications. Sarlink ME-2365B is a medium hardness, low density, UV stabilized, high flow grade delivering excellent aesthetics and faster injection molding cycle times.
General Information
Features
  • Low Specific Gravity
  • Sunlight Resistant
  • Low density
  • Light stabilization
  • Good UV resistance
  • Workability, good
  • Fast molding cycle
  • Good adhesion
  • High liquidity
  • Good chemical resistance
  • Lubrication
  • Excellent appearance
  • Medium hardness
Uses
  • Application in Automobile Field
  • Automotive exterior parts
  • Car exterior decoration
  • Rubber substitution
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 0.890g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)15g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ISO 868
    Shore A, 1 second, injection molding 69ISO 868
    Shore A, 5 seconds, injection molding 65ISO 868
    Shore A, 15 seconds, injection molding 64ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress 1ISO 37
    Transverse flow : 100% strain 1.70MPaISO 37
    Flow : 100% strain 2.00MPaISO 37
Tensile Stress 2ISO 37
    Transverse flow : Fracture 10.5MPaISO 37
    Flow : Fracture 5.80MPaISO 37
Tensile Elongation 3ISO 37
    Transverse flow : Fracture 880%ISO 37
    Flow : Fracture 710%ISO 37
Tear Strength 4ISO 34-1
    Transverse flow 28kN/mISO 34-1
    Flow 27kN/mISO 34-1
Compression Set 5ISO 815
    23°C, 22 hr 24%ISO 815
    70°C, 22 hr 39%ISO 815
    90°C, 70 hr 63%ISO 815
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air - Across Flow 6ISO 188
    110°C, 1008 hr -9.8%ISO 188
    100% strain 110°C, 1008 hr 13%ISO 188
    125°C, 168 hr -11%ISO 188
    100% strain 125°C, 168 hr 15%ISO 188
Changes in tensile stress upon fracture in air- Transverse flow 7ISO 188
    110°C, 1008 hr 1.3%ISO 188
    125°C, 168 hr -1.3%ISO 188
Change in Shore Hardness in Air 8ISO 188
    Shao A, 110°C, 1008 hr 2.8ISO 188
    Shao A, 125°C, 168 hr 1.7ISO 188
Fill AnalysisNominal ValueUnitTest Method
Apparent Viscosity (200°C, 206 sec^-1)134Pa·sASTM D3835
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 199 - 210°C
Middle Temperature 204 - 216°C
Front Temperature 210 - 221°C
Nozzle Temperature 216 - 227°C
Processing (Melt) Temp 216 - 227°C
Mold Temperature 35 - 66°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Fast
Back Pressure 0.172 - 0.862MPa
Screw Speed 50 - 120rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
Note Message
1 .Type 1, 510mm/min
2 .Type 1, 510mm/min
3 .Type 1, 510mm/min
4 .B method, right angle specimen (without cut), 510mm/min
5 .Type a
6 .Type 1
7 .Type 1
8 .5 sec
Resin Grade Manufacturer Category Trademark
Bergamid™ A70 G30 Black PolyOne Corporation Nylon 66 Bergamid™
BLUESTAR® POM BS270A Beijing Ranger Chemical Co., Ltd. Acetal (POM) Copolymer BLUESTAR® POM
CoREZYN® COR30-DA-250 Interplastic Corporation Polyester, TS CoREZYN®
Kumho KTR KTR-401H Korea Kumho Petrochemical Co., Ltd. SBS Kumho KTR
Sylvin 802-80 Clear 876 Sylvin Technologies Incorporated PVC, Unspecified Sylvin