| Category: | ABS , Acrylonitrile Butadiene Styrene |
| Manufacturer: | Polimarky Spolka Jawna |
| Trademark: | Restren |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | grWwlQ_Restren-ABS.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Restren ABS is an Acrylonitrile Butadiene Styrene (ABS) product. It is available in Europe. |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.03 to 1.06 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 25 to 45 | g/10 min |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2000 to 2300 | MPa | ISO 527-2 |
| Tensile Stress | 39.0 to 45.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.0 to 30 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 16 to 26 | kJ/m² | ISO 179/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 94.0 to 98.0 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 102 to 104 | °C | ISO 306/A120 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 to 85.0 | °C | |
| Drying Time | 3.0 | hr | |
| Processing (Melt) Temp | 220 to 250 | °C | |
| Mold Temperature | 40.0 to 70.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Epocast 1622 FST A/B | Huntsman Advanced Materials | Epoxy | Epocast |
| Iupiace® LV60 | Mitsubishi Engineering-Plastics Corp | PPE+PS | Iupiace® |
| Plaslube® PA6/6 GF30 X | Techmer Engineered Solutions | Nylon 66 | Plaslube® |
| TECHNYL STAR® S 60G1 V30 GREY R7012 | Solvay Engineering Plastics | Nylon 6 | TECHNYL STAR® |
| LNP™ LUBRICOMP™ Lexan_LF1520A compound | SABIC Innovative Plastics | PC | LNP™ LUBRICOMP™ |