Category: | PP Homopolymer , Polypropylene Homopolymer |
Manufacturer: | Polykemi AB |
Trademark: | POLYfill |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gdWZe8_POLYfill-PPH-GF8020-PD2.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre-reinforced Chemically coupled |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.05 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 8.0 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.60 to 0.80 | % | |
Flow | 0.30 to 0.40 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 80.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 4.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 4300 | MPa | ISO 178 |
Flexural Stress | 110 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 5.0 | kJ/m² | |
23°C | 8.0 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 150 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 130 | °C | ISO 75-2/A |
Vicat Softening Temperature | 125 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 201 MS 2 HB | RTP Company | Nylon 66 | RTP |
Roscom PVC 201LFR-65 Natural | Roscom, Inc. | PVC, Flexible | Roscom PVC |
Flontech® FT-1-FM-5 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
Ecomass® 1850ZN66T1 | Ecomass Technologies | Nylon 6 | Ecomass® |
Wanthane® WHT-1189B | Wanhua Chemical Group Co., Ltd. | TPU-Polyester | Wanthane® |