| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | Baoding Bangtai Polymeric New-Materials Co.,Ltd |
| Trademark: | Baoding |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | RpOq25_Baoding-76T90.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Properties: Outstanding weather and cold resistance, hydrolysis resistance and good flexibility at low temperature. Application: Soft oil hoses,Oil pipes, Shale gas hoses, Protective cover for signal transmission line, Fire hose linings, Sea recreational equipments. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.10 to 1.14 | g/cm³ | JIS K7311 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A) | 88 to 92 | JIS K7311 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | JIS K7311 | ||
| 100% Strain | 10.8 | MPa | |
| 300% Strain | 22.6 | MPa | |
| Tensile Strength | 30.4 | MPa | JIS K7311 |
| Tensile Elongation (Break) | 380 | % | JIS K7311 |
| Tear Strength | 130 | kN/m | JIS K7311 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 100 | °C | |
| Drying Time | 3.0 to 5.0 | hr | |
| Processing (Melt) Temp | 180 to 220 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Techsil 1387 BLACK | Techsil Limited | Silicone | Techsil |
| Weatherflex™ CS1521WX NTL01B | Colorite Polymers | PVC, Flexible | Weatherflex™ |
| NOVAREX® M7026U | Mitsubishi Engineering-Plastics Corp | PC | NOVAREX® |
| Fluon® PTFE PB1202 | Asahi Glass Co., Ltd. | PTFE | Fluon® |
| EcoLon® MRGF1518-BK | Wellman Engineering Resins | Nylon 66 | EcoLon® |