Ultramid® T KR 4355 G8 FC BK23262

Category: Nylon 6/6T , Polyamide 6/6T Copolymer
Manufacturer: BASF Corporation
Trademark: Ultramid®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: GV5OQ0_Ultramid-T-KR-4355-G8-FC-BK23262.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
The BASF Ultramid® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including FDA, European Food Contact (EU) Nr. 11/2011 and GMP (EC) n°2023/2006.

Additional food contact compliances may also be available. Please contact your local representative or plastics safety (E-Mail: plastics.safety@basf.com, Fax: +49 621-60-93253).
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 40% filler by weight
Features
  • Compliance of Food Exposure
Uses
  • Non-specific food applications
Agency Ratings
  • EC 1907/2006 (REACH)
  • EC 2023/2006
  • FDA Food Exposure, Not Rated
  • European food contact, not rated
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.50g/cm³ISO 1183
Molding Shrinkage ISO 294-4
    Vertical flow direction 0.90%ISO 294-4
    Flow direction 0.30%ISO 294-4
Mold Shrinkage - constrained 10.45%
ThermalNominal ValueUnitTest Method
Maximum operating temperature- short cycle operation 260°C
InjectionNominal ValueUnit
Screw Speed mm/sec
MechanicalNominal ValueUnitTest Method
Tensile Modulus 13500MPaISO 527-2
Tensile Stress (Break)230MPaISO 527-2
Tensile Strain (Break)2.5%ISO 527-2
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength (23°C)9.0kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)80kJ/m²ISO 179/1eU
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)250°CISO 75-2/A
Melting Temperature 294°CISO 11357-3
InjectionNominal ValueUnit
Drying Temperature 110°C
Drying Time 8.0hr
Suggested Max Moisture 0.15%
Hopper Temperature 80.0°C
Rear Temperature 300°C
Middle Temperature 310°C
Front Temperature 320°C
Nozzle Temperature 320°C
Processing (Melt) Temp 310 - 330°C
Mold Temperature 80.0 - 120°C
Injection instructions
Residence Time: <10 min.
Note Message
1 .Test box with central gating, dimensions of base (107*47*1,5) mm, processing condition: TM = 320°C (unreinforced) or 330°C (reinforced), TW = 80°C
Resin Grade Manufacturer Category Trademark
tefanyl® VE VEEP 115 Mitsubishi Chemical Performance Polymers, Inc. PVC+NBR tefanyl® VE
VITAMIDE® BF13RD6339 Jackdaw Polymers Nylon 6 VITAMIDE®
Iupilon® GPX2010PH Mitsubishi Engineering-Plastics Corp PC Iupilon®
PENTAMID AB S GV50 H black PENTAC Polymer GmbH Nylon 66/6 PENTAMID AB
Sylvin 9067F3 Red 6270 Sylvin Technologies Incorporated PVC, Unspecified Sylvin