| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | G7THhY_Chemlon-230-GH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Chemlon® 230 GH is a Polyamide 6 (Nylon 6) material filled with 30% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon® 230 GH: Flame Rated. Typical application of Chemlon® 230 GH: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.36 | g/cm³ | ISO 1183 |
| Molding Shrinkage 1 | 0.15 to 0.40 | % | ISO 294-4 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 158 | MPa | ISO 527-2 |
| Tensile Strain | ISO 527-2 | ||
| Yield | 3.0 | % | |
| Break | 3.0 | % | |
| Flexural Modulus | 8100 | MPa | ISO 178 |
| Flexural Stress | 225 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | ISO 180/1A | ||
| -40°C | 9.0 | kJ/m² | |
| 23°C | 11 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 200 | °C | ISO 75-2/A |
| Melting Temperature | 220 | °C | ASTM D789 |
| CLTE - Flow | 5.3E-5 | cm/cm/°C | ASTM D696 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+15 | ohms·cm | ISO 1325 |
| Dielectric Strength (3.00 mm) | 11 | kV/mm | ASTM D149 |
| Comparative Tracking Index | > 600 | V | Internal Method |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.810 mm) | HB | UL 94 | |
| Oxygen Index | 22 | % | ISO 4589-2 |
| FMVSS Flammability | Passed | FMVSS 302 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Suggested Max Moisture | 0.20 | % | |
| Suggested Max Regrind | 25 | % | |
| Rear Temperature | 235 to 245 | °C | |
| Middle Temperature | 245 to 260 | °C | |
| Front Temperature | 245 to 270 | °C | |
| Nozzle Temperature | 245 to 270 | °C | |
| Processing (Melt) Temp | 245 to 270 | °C |
| Note Message | |
|---|---|
| 1 . | Dependent upon molding conditions particularly Mold temperature. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 MS 5 | RTP Company | Nylon 66 | RTP |
| Sylvin 9067F5 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ADEKA ED-505 | Adeka Corporation | Epoxy | ADEKA |
| Evoprene™ COGEE 626 | AlphaGary | SEBS | Evoprene™ COGEE |
| LNP™ THERMOCOMP™ KZ002 compound | SABIC Innovative Plastics | Acetal (POM) Copolymer | LNP™ THERMOCOMP™ |