Thermoplastic Elastomer Vulcanized. This TPE-V compound combines the typical performance of a vulcanized elastomer with the easy processing of a thermoplastic compound. Taroprene is totally recyclable and it can be produced in standard grades and in tailor-made grades. Available in natural, black and colored grade. |
General Information | |
---|---|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 3.0 | g/10 min | ISO 1133 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A, 3 sec) | 70 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1 | ASTM D412 | ||
100% Strain | 3.00 | MPa | |
300% Strain | 5.10 | MPa | |
Tensile Strength 2(Break) | 6.80 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 480 | % | ASTM D412 |
Tear Strength | 25.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
70°C, 22 hr | 35 | % | |
100°C, 22 hr | 40 | % |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 170 to 230 | °C |
Note Message | |
---|---|
1 . | Die C |
2 . | Die C |
3 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Reslen PPH 50GF | Polimarky Spolka Jawna | PP Homopolymer | Reslen |
Staramide BST43 | Eurostar Engineering Plastics | Nylon 6 | Staramide |
TAROPRENE® 1 A60 M1M | Taro Plast S.p.A. | TPV | TAROPRENE® |
ACCUTECH™ HP0334T30L | ACLO Compounders Inc. | PP Homopolymer | ACCUTECH™ |
LUVOCOM® 1-0936-3 | Lehmann & Voss & Co. | Nylon 66 | LUVOCOM® |