| Evoprene™087 is a thermoplastic elastomer (TPE) product,. It can be processed by extrusion or injection molding and is available in North America or Europe. Evoprene™The application areas of 087 include wire and cable, engineering/industrial accessories, sealing applications, automotive industry and handles. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.10 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 61 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break) | 5.80 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 620 | % | ISO 527-2 |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Trouser Tear Resistance | 30.0 | N/mm | ISO 6383-1 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (300% Strain) | 2.30 | MPa | ISO 37 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 21 | % | ISO 815 |
| 70°C, 22 hr | 73 | % | ISO 815 |
| 100°C, 22 hr | 89 | % | ISO 815 |
| Additional Information |
|---|
| Abrasion Resistance, DIN 53516: 256 mm³ lossOzone Resistance, ISO 1431, 100 pphm/200hrs/20% strain: No CracksUV Resistance, 2250 hrs Xenon: GoodHardness Change, ISO 188, Heat Aged 14 Days @ 70°F: -1Retained T/S, ISO 188, Heat Aged 14 Days @ 70°F: 104%Retained E/B, ISO 188, Heat Aged 14 Days @ 70°F: 104%Service Temperature: -55 to 140°FThe value listed as Density, ISO 1183, was tested in accordance with ISO 2781.The value listed as Stress @ Break, ISO 527-1, was tested in accordance with ISO 37.The value listed as Strain @ Break, ISO 527-1, was tested in accordance with ISO 37. |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Processing (Melt) Temp | 160 - 179 | °C | |
| Mold Temperature | 16 - 29 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | 129 - 149 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shanghai Potomer N-500 | Shanghai Potomer International Trade Co., Ltd. | CPVC | Shanghai Potomer |
| Badaflex® TPE-S 50A 1000LD | Bada AG | TPE | Badaflex® |
| DSR TLE-102 | Dragon Special Resin (Xiamen) Co., Ltd. | PET | DSR |
| Infino SC-1220R | SAMSUNG SDI CO., LTD. | PC | Infino |
| Magnobond 92-1 | Magnolia Plastics, Inc. | Epoxy | Magnobond |