| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Polykemi AB |
| Trademark: | SCANAMID 66 |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | zoau6p_SCANAMID-66-A33-E-F45.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre reinforced Elastomer modified |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.48 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 0.80 | % | |
| Flow | 0.30 | % | |
| Viscosity | High | Pa·s |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 150 | MPa | ISO 527-2 |
| Tensile Strain | ISO 527-2 | ||
| Yield | 3.7 | % | |
| Break | 4.5 | % | |
| Flexural Modulus (23°C) | 11000 | MPa | ISO 178 |
| Flexural Stress | 250 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -20°C | 14 | kJ/m² | |
| 23°C | 20 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179 | ||
| -20°C | No Break | ||
| 23°C | No Break |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(1.8 MPa, Unannealed) | 230 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 240 | °C | ISO 306/B50 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Santoprene™ 8271-55 | ExxonMobil Chemical | TPV | Santoprene™ |
| MOSTEN GB 503 | UNIPETROL RPA | PP Copolymer | MOSTEN |
| ACCULOY™ PCA083L | ACLO Compounders Inc. | PC+ABS | ACCULOY™ |
| KOPA® KN133G33HIBL | Kolon Plastics, Inc. | Nylon 6 | KOPA® |
| ICORENE® N9205 | ICO Polymers EMEA, A Division of A. Schulman | PET | ICORENE® |