| Category: | Nylon+PP , Polyamide + PP |
| Manufacturer: | A. Schulman Europe |
| Trademark: | SCHULABLEND® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | znzocf_SCHULABLENDPAPPMMO7101GF25.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 25% glass fibre reinforced PA6/PP blend with excellent chemical resistance |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Processing Method |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.20 | g/cm³ | ISO 1183/A |
| Melt Volume-Flow Rate (MVR) (250°C/2.16 kg) | 4.00 | cm³/10min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Ball Indentation Hardness (H 358/30) | 108 | MPa | ISO 2039-1 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 6700 | MPa | ISO 527-2/1A/1 |
| Tensile Stress (Break) | 103 | MPa | ISO 527-2/1A/5 |
| Tensile Strain (Break) | 3.0 | % | ISO 527-2/1A/5 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -30°C | 6.0 | kJ/m² | ISO 179/1eA |
| 23°C | 10 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength | ISO 179/1eU | ||
| -30°C | 55 | kJ/m² | ISO 179/1eU |
| 23°C | 45 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 184 | °C | ISO 75-2/Bf |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | > 1.0E+15 | ohms | IEC 60093 |
| Volume Resistivity | > 1.0E+13 | ohms·cm | IEC 60093 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flammability Classification (1.6 mm) | HB | IEC 60695-11-10, -20 |
| Additional Information |
|---|
| 1.) Not for use in food contact applications2.) Not for use in medical or pharmaceutical applications |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80 | °C | |
| Drying Time | 3.0 - 4.0 | hr | |
| Suggested Max Moisture | 0.040 - 0.10 | % | |
| Processing (Melt) Temp | 240 - 270 | °C | |
| Mold Temperature | 60 - 90 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RABALON® PJ7300C | Mitsubishi Chemical Performance Polymers, Inc. | TPE | RABALON® |
| Wellamid® XT1486-BK | Wellman Engineering Resins | Nylon 66 | Wellamid® |
| APEX® 85-J438D-6 | Teknor Apex Company | PVC, Flexible | APEX® |
| Cheng Yu IPS620BK | Cheng Yu Plastic Company Limited | PS (HIPS) | Cheng Yu |
| ENFLEX VU-420-60A | Ravago Group | PP+EPDM | ENFLEX |