| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | AlphaGary |
| Trademark: | SMOKEGUARD™ V |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | zVDE9I_SMOKEGUARD-V-1118-NATURAL.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| A LOW SMOKE, HIGHLY FLAME RETARDED, 75°C DEGREE, LEAD FREE SMOKEGUARD JACKETING COMPOUND FOR PLENUM CABLE CONSTRUCTIONS. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.55 to 1.59 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shore D | 67 to 73 | ||
| Shore D, 15 sec | 53 to 59 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D412 | ||
| 0.381 mm | 17.2 | MPa | |
| 1.91 mm | 15.2 | MPa | |
| Tensile Elongation | ASTM D412 | ||
| Break, 1.91 mm | 210 | % | |
| Break, 0.381 mm | 190 | % |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -6.00 | °C | ASTM D746 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Dielectric Constant (23°C, 100 MHz) | 3.50 | ASTM D150 | |
| Dissipation Factor (23°C, 100 MHz) | 0.018 | ASTM D150 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index (3.18 mm) | 50 | % | ASTM D2863 |
| Smoke | 3.0 | % | ASTM D4100 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Wellamid® MRGF25/15 42H-NR | Wellman Engineering Resins | Nylon 6 | Wellamid® |
| Hylon® N7243HL | Ravago Manufacturing Americas, LLC | Nylon 6/12 | Hylon® |
| Idemitsu PS IT43 | Idemitsu PS | PS (GPPS) | Idemitsu PS |
| LNP™ STAT-KON™ DX09315C compound | SABIC Innovative Plastics Asia Pacific | PC | LNP™ STAT-KON™ |
| Shida 030E-1 | JINJIANG City SHIDA Plastic Fine Co., Ltd. | SBS | Shida |