| Category: | Silicone , Silicone |
| Manufacturer: | Synres-Almoco BV |
| Trademark: | Synres-Almoco |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | zCcGXG_Synres-Almoco-SI-4554.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Glass-fibre reinforced silicone compound Excellent thermal stability - continual use temperatures of up to 300 °C, exceptional electrical properties, good mechanical strength, very good dimensional stability Primary application(s): Very high heat resistant connectors This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS) |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 2.10 to 2.20 | g/cm³ | ISO 1183 |
| Apparent Density | 0.95 to 1.05 | g/cm³ | ISO 60 |
| Molding Shrinkage - Flow | ISO 2577 | ||
| -- 1 | 0.40 to 0.80 | % | |
| -- 2 | 0.20 to 0.60 | % | |
| Water Absorption (23°C, 24 hr) | < 0.10 | % | ISO 62 |
| Post Shrinkage 3 | < 0.050 | % | ISO 2577 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus (Injection Molded) | 5000 to 6000 | MPa | ISO 527-2 |
| Tensile Stress (Injection Molded) | 20.0 to 30.0 | MPa | ISO 527-2 |
| Flexural Modulus (Injection Molded) | 12000 to 16000 | MPa | ISO 178 |
| Flexural Stress (Injection Molded) | 60.0 to 80.0 | MPa | ISO 178 |
| Compressive Stress | 70.0 to 90.0 | MPa | ISO 604 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (Injection Molded) | 2.0 to 3.5 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength (Injection Molded) | 4.0 to 6.0 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 1.8 MPa, Unannealed | > 200 | °C | ISO 75-2/A |
| 8.0 MPa, Unannealed | > 200 | °C | ISO 75-2/C |
| CLTE - Flow (50 to 150°C) | 2.0E-5 to 4.0E-5 | cm/cm/°C | ISO 11359-2 |
| Thermal Conductivity | 0.40 to 0.60 | W/m/K | ASTM E1461 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+13 to 1.0E+14 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+14 to 1.0E+15 | ohms·cm | IEC 60093 |
| Electric Strength | 20 to 30 | kV/mm | IEC 60243-1 |
| Relative Permittivity | IEC 60250 | ||
| 100 Hz | 6.00 4.00 | ||
| 1 MHz | 6.00 4.00 | ||
| Dissipation Factor | IEC 60250 | ||
| 100 Hz | 0.010 to 0.020 | ||
| 1 MHz | 5.0E-3 to 0.010 | ||
| Arc Resistance | PLC 4 | ASTM D495 | |
| Comparative Tracking Index | > 350 | V | IEC 60112 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.600 mm, Tested by RASCHIG) | V-0 | UL 94 |
| Note Message | |
|---|---|
| 1 . | Compression Molded |
| 2 . | Injection Molded |
| 3 . | 168 h / 110°C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Monprene® CE-22068 | Teknor Apex Company | TPE | Monprene® |
| TECAPEEK® GF30 | Ensinger Inc. | PEEK | TECAPEEK® |
| ALFATER XL® A60I 3EF0001 | ALBIS PLASTIC GmbH | TPV | ALFATER XL® |
| Generic POP | Generic | POP | Generic |
| Sylvin 8200-85 White 1519 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |