Category: | LLDPE , Linear Low Density Polyethylene |
Manufacturer: | Saudi Basic Industries Corporation (SABIC) |
Trademark: | SABIC® LLDPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | yvqMd3_SABICLLDPE118WE.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
SABIC® LLDPE 118WE is a butene-linear low density polyethylene resin for general purpose applications. Films produced from this resin are tough with excellent puncture resistance, high tensile strength, good hottack properties and low gel levels. The resin contains anti block and slip erucamide. SABIC® LLDPE 118WE is TNPP free. Application Typical applications for SABIC® LLDPE 118WE are shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE. The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/medical applications. |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.918 | g/cm³ | ISO 1183/A |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 1.0 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Coefficient of Friction (Blown Film) | 0.10 | ISO 8295 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Film Thickness - Tested | 50 | µm | |
Tensile Modulus | ISO 527-3 | ||
MD : 50 µm, blown film | 160 | MPa | ISO 527-3 |
TD : 50 µm, blown film | 180 | MPa | ISO 527-3 |
Tensile Stress | ISO 527-3 | ||
MD : Yield, 50 µm, blown film | 11.0 | MPa | ISO 527-3 |
TD : Yield, 50 µm, blown film | 11.0 | MPa | ISO 527-3 |
MD : Broken, 50 µm, blown film | 37.0 | MPa | ISO 527-3 |
TD : Broken, 50 µm, blown film | 30.0 | MPa | ISO 527-3 |
Tensile Elongation | ISO 527-3 | ||
MD : Broken, 50 µm, blown film | 600 | % | ISO 527-3 |
TD : Broken, 50 µm, blown film | 800 | % | ISO 527-3 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Impact Strength - Blown Film (50.0 µm) | 220 | J/cm | ASTM D4272 |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Clarity - Blown Film (50.0 µm) | 0.0200 | V | Internal method |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Blocking - Blown Film (50.0 µm) | 15 | g | Internal method |
Puncture Resistance - Blown Film (50.0 µm) | 380 | J/m | Internal method |
Re-blocking - Blown Film (50.0 µm) | 10 | g | Internal method |
Tear Strength 1 | ISO 6383-2 | ||
MD : 50.0 µm | 40.0 | kN/m | ISO 6383-2 |
TD : 50.0 µm | 120.0 | kN/m | ISO 6383-2 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 101 | °C | ISO 306/A |
Melting Temperature (DSC) | 121 | °C | Internal method |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Gloss (45°, 50.0 µm, Blown Film) | 42 | ASTM D2457 | |
Haze (50.0 µm, Blown Film) | 20 | % | ASTM D1003A |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Film of 50 µm and BUR=2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2,7 mm. |
Note Message | |
---|---|
1 . | Blown Film |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
polyvic® M-1868-GL 06 | Unipack Plasindo | PVC, Unspecified | polyvic® |
RTP 800 AR 15 TFE 13 SI 2 | RTP Company | Acetal (POM) Copolymer | RTP |
Wellamid® FRGF1827-BK1 | Wellman Engineering Resins | Nylon 66 | Wellamid® |
ExTima™ GP MB PP 120 | Ovation Polymers Inc. | PP, Unspecified | ExTima™ |
Petrothene® NA952094 | LyondellBasell Industries | LDPE | Petrothene® |