Staramide RF008U

Category: Nylon 66/6 , Polyamide 66/6 Copolymer
Manufacturer: Eurostar Engineering Plastics
Trademark: Staramide
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: yu3GAF_Staramide-RF008U.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Staramide RF008U a 40 % Glass Fiber Reinforced Polyamide 66 / Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)
General Information
Filler / Reinforcement
  • Glass Fiber, 40% Filler by Weight
RoHS Compliance
  • RoHS Compliant
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.46g/cm³ISO 1183
Molding Shrinkage - Flow (4.00 mm)0.20 to 0.40%Internal Method
MechanicalNominal ValueUnitTest Method
Tensile Stress (Break)189MPaISO 527-2/5
Tensile Strain (Break)2.3%ISO 527-2/5
Flexural Modulus 111000MPaISO 178
Flexural Stress 276MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength 2(23°C)14kJ/m²ISO 180/1A
Unnotched Izod Impact Strength 3(23°C)70kJ/m²ISO 180/1U
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature 4(1.8 MPa, Unannealed, 64.0 mm Span)258°CISO 75-2/Af
CLTE - Flow (23 to 60°C)2.7E-5cm/cm/°CISO 11359-2
InjectionNominal ValueUnit
Drying Temperature 75.0 to 85.0°C
Drying Time 4.0 to 6.0hr
Suggested Max Moisture 0.20%
Rear Temperature 260 to 280°C
Middle Temperature 270 to 280°C
Front Temperature 270 to 290°C
Processing (Melt) Temp 270 to 290°C
Mold Temperature 60.0 to 90.0°C
Note Message
1 .2.0 mm/min
2 .80*10*4
3 .80*10*4
4 .80*10*4
Resin Grade Manufacturer Category Trademark
RTP 207 A TFE 13 SI 2 RTP Company Nylon 6 RTP
TECHNOGRAN® PCI BLK Eurocompound Polymers PC TECHNOGRAN®
AMTOPP BA30 Inteplast Group PP, Unspecified AMTOPP
Globalene® ST751 Lee Chang Yung Chemical Industry Corp. PP Impact Copolymer Globalene®
Lumid® HI2202B(W) LG Chem Ltd. Nylon 66 Lumid®