| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | EMAS Plastik San.Tic.AS. |
| Trademark: | NYLEM® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | yrGYIW_NYLEM-6-GXR-20.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyamide 6, %20 glass fiber/beads reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.24 to 1.28 | g/cm³ | ISO 1183 |
| Molding Shrinkage | 0.35 to 0.45 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 75 to 80 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5000 to 8000 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 100 to 130 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 5.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | > 6.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 205 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 215 | °C | ISO 306/B |
| Melting Temperature (DSC) | 220 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shin-Etsu Elastomer X-30-783U | Shin-Etsu Silicones of America | Silicone Rubber, HTV | Shin-Etsu Elastomer |
| Sylvin 8208-78 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ALCUDIA® EVA PA-430 | REPSOL | EVA | ALCUDIA® EVA |
| Boda BDF-KK2802 | Chenguang Fluoro & Silicone Elastomers Co., Ltd. | Fluorelastomer | Boda |
| LEXAN™ FXG1414T resin | SABIC Innovative Plastics | PC | LEXAN™ |