SPI 1029 BK is a Polyamide 6 (Nylon 6) product filled with 20% glass fiber. It is available in North America. Characteristics include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.25 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 0.20 to 0.60 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 5170 to 6210 | MPa | ASTM D638 |
Tensile Strength (Yield) | 86.2 to 103 | MPa | ASTM D638 |
Tensile Elongation (Yield) | 2.0 to 5.0 | % | ASTM D638 |
Flexural Modulus | 4650 to 5580 | MPa | ASTM D790 |
Flexural Strength | 127 to 152 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 80 to 120 | J/m | ASTM D256 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.50 mm) | HB | Internal Method |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 82.2 | °C | |
Drying Time - Desiccant Dryer | 2.0 to 6.0 | hr | |
Dew Point | -17.8 | °C | |
Suggested Max Moisture | 0.20 | % | |
Processing (Melt) Temp | 243 to 279 | °C | |
Mold Temperature | 54.4 to 93.3 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MAJORIS UG500 - 8229 | AD majoris | Nylon 66 | MAJORIS |
RJM SB302G15 | RJM International, Inc. | PBT | RJM |
Starex WR-9130 | SAMSUNG SDI CO., LTD. | ASA | Starex |
VICTREX® PEEK 600G | Victrex plc | PEEK | VICTREX® PEEK |
Generic PC+PBT | Generic | PC+PBT | Generic |