Andur 1-83 AP/Curene® 442

Category: PUR-Ether/TDI , Polyurethane (Polyether, TDI)
Manufacturer: Anderson Development Company
Trademark: Andur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: yXh9bR_Andur-1-83-AP-Curene-442.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Andur 1-83 AP is a polyether (PTMG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 83-85 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by curing Andur 1-83 AP with polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.07g/cm³ASTM D1505
Molding Shrinkage - Flow 1.3%ASTM D955
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)84ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 4.69MPaASTM D412
    300% strain 8.27MPaASTM D412
Tensile Strength (Yield)31.7MPaASTM D412
Tensile Elongation (Break)550%ASTM D412
Bayshore Resilience 56%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 8.0 - 11min
Demold Time 30min
Post Cure Time (96°C)16hr
Additional Information
Durometer Hardness, ASTM D2240, Shore A: 83 to 85Die C Tear, ASTM D1004: 350 pliAverage Split Tear, ASTM D1938: 70 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 1-83 AP: 160-180°F Curene 442: 230-240°F
InjectionNominal ValueUnit
Mold Temperature 100 - 113°C
Resin Grade Manufacturer Category Trademark
Trexprene® A40NI-HF Mitsubishi Chemical Performance Polymers, Inc. TPV Trexprene®
Elastron® G G601.A80.N Elastron USA, Inc. SEBS Elastron® G
Karina IVORY PVC COMPOUND 70900-35/ 1-A-AC-LF (*) Karina Ind. e Com. de Plásticos Ltda PVC, Unspecified Karina
RTP 399 X 141379 A RTP Company PC RTP
ESTOPLAST XU 430NN01 Ester Industries Ltd. Nylon 6 ESTOPLAST XU