Elastollan® S95AN

Category: TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester)
Manufacturer: BASF Corp. Thermoplastic Polyurethanes
Trademark: Elastollan®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: yRSkok_Elastollan-S95AN.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Elastollan® S95AN is specifically formulated for injection molding applications with short cycling time. It exhibits good hydrolytic stability, excellent abrasion resistance, toughness, good heat, oil, fuel, and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® S95AN is supplied uncolored in diced form.
General Information
Features
  • Good Abrasion Resistance
  • Good Tear Strength
  • Good Toughness
  • High Heat Resistance
  • Hydrolytically Stable
  • Solvent Resistant
Appearance
  • Colorless
Processing Method
  • Extrusion
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.23g/cm³ASTM D792
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore A 93
    Shore D 47
MechanicalNominal ValueUnitTest Method
Tensile Modulus (Injection Molded)82.7MPaASTM D412
Flexural Modulus (Injection Molded)75.8MPaASTM D790
Taber Abrasion Resistance 30.0mgASTM D1044
Abrasion - DIN 30mm³DIN 53516
ThermalNominal ValueUnitTest Method
Softening Point - DMA 142°CInternal Method
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% Strain 15.9MPa
    300% Strain 33.1MPa
Tensile Strength 45.5MPaASTM D412
Tensile Elongation (Break)500%ASTM D412
Tear Strength 1166kN/mASTM D624
Compression Set ASTM D395B
    23°C, 22 hr 25%
    70°C, 22 hr 45%
ThermalNominal ValueUnitTest Method
Glass Transition Temperature -22.0°CInternal Method
Vicat Softening Temperature 145°CASTM D1525
InjectionNominal ValueUnit
Drying Temperature 110 to 120°C
Drying Time 2.0 to 3.0hr
Suggested Max Moisture 0.030%
Rear Temperature 190 to 220°C
Middle Temperature 190 to 220°C
Front Temperature 190 to 220°C
Nozzle Temperature 210 to 225°C
ExtrusionNominal ValueUnit
Drying Temperature 110 to 120°C
Drying Time 2.0 to 3.0hr
Cylinder Zone 1 Temp. 170 to 210°C
Cylinder Zone 3 Temp. 170 to 210°C
Cylinder Zone 5 Temp. 170 to 210°C
Adapter Temperature 200 to 220°C
Die Temperature 195 to 215°C
Note Message
1 .Die C
Resin Grade Manufacturer Category Trademark
Tenac™-C Z4520 Asahi Kasei Chemicals Corporation Acetal (POM) Copolymer Tenac™-C
SUSTAMID 6G PD 140 Röchling Sustaplast SE & Co. KG Nylon 6 SUSTAMID
Vipel® F701-SPT-30 AOC, L.L.C. Polyester Alloy Vipel®
ADDINYL B2 V15 ADDIPLAST Nylon 6 ADDINYL
KumhoSunny PC/ABS HAC6020FG Shanghai KumhoSunny Plastics Co., Ltd. PC+ABS KumhoSunny PC/ABS