GETILAN is our trade-mark of our crosslinkable polythene. GETILAN GPE/452 BLACK is a high density chemically crosslinkable polythene for insulated aerial cables It is a conveniently grafted polythene able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/203 HS. REACTION BETWEEN GRAFTING AND CATALYST: These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5 |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.950 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 0.20 - 0.60 | g/10 min | ASTM D1238 |
Carbon Black Content | 2.5 | % |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Thermoset 1 | IEC 60811 | ||
150°C | % | IEC 60811 | |
Residual : 150°C | 0.00 | IEC 60811 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 20.0 | MPa | IEC 60811 |
Tensile Strain (Break) | 430 | % | IEC 60811 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air | IEC 60811 | ||
127°C, 40 hr | 10 | % | IEC 60811 |
150°C, 240 hr | 10 | % | IEC 60811 |
Change in Tensile Strain at Break in Air | IEC 60811 | ||
127°C, 40 hr | -5.0 | % | IEC 60811 |
150°C, 240 hr | -20 | % | IEC 60811 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+16 | ohms·cm | BS 6622 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 165 | °C | |
Cylinder Zone 2 Temp. | 180 | °C | |
Cylinder Zone 3 Temp. | 190 | °C | |
Cylinder Zone 4 Temp. | 205 | °C | |
Cylinder Zone 5 Temp. | 210 | °C | |
Die Temperature | 225 | °C |
Extrusion instructions |
---|
CROSSLINKING:Crosslinking of the finished product is obtained by: Immersion of the bobbin in hot water at 85/90°C for two hours (up to 3 mm thickness) Steam treatment at 0.15 bar for 5/6 hours. Air crosslinking at natural temperatures and moisture, after a right number of days depending on climatic conditions, is possibile. |
Note Message | |
---|---|
1 . | 40 N/cm² |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SITRALON 15E-UV-V0 / C9180 weiss | SITRAPLAS GmbH | PC | SITRALON |
Varcum 29457 | Durez Corporation | Phenolic | Varcum |
NuSil CV4-2289-1 | NuSil Technology | Silicone | NuSil |
ExxonMobil™ LDPE EVA Copolymers LD 361 Series | ExxonMobil Chemical | LDPE | ExxonMobil™ LDPE |
Electrafil® ABS 03011 FR BK MB | Techmer Engineered Solutions | ABS | Electrafil® |