Message |
---|
Polyamide 66, %30 glass beads reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Recycled Content |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.32 to 1.36 | g/cm³ | ISO 1183 |
Molding Shrinkage | 0.45 to 0.55 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D) | 80 to 85 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 5000 to 8000 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 140 to 170 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 3.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | > 10 | kJ/m² | ISO 180/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 250 | °C | ISO 75-2/A |
Vicat Softening Temperature | 240 | °C | ISO 306/B |
Melting Temperature (DSC) | 265 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
POLYVIN® PVC 6620 | A. Schulman Inc. | PVC, Unspecified | POLYVIN® |
Tefzel® 750 | DuPont Fluoropolymers | ETFE | Tefzel® |
Nycal™ 2050R10 | Technical Polymers, LLC | Nylon 612 | Nycal™ |
LUVOCOM® 80-7388 | Lehmann & Voss & Co. | Acetal (POM) Copolymer | LUVOCOM® |
Osterlene® HI-13-2.1 | Osterman & Company | PS (HIPS) | Osterlene® |