Glass Fiber - PTFE Lubricated
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 35% filler by weight
Additive
  • PTFE lubricant (15%)
Features
  • Lubrication
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.54g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.15 - 0.40%ASTM D955
Moisture Content 0.20%
Additional InformationNominal ValueUnit
Primary Additive 35%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 11400MPaASTM D638
Tensile Strength 155MPaASTM D638
Tensile Elongation (Yield)2.5 - 4.5%ASTM D638
Flexural Modulus 10300MPaASTM D790
Flexural Strength 241MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)110J/mASTM D256
Unnotched Izod Impact (3.20 mm)960J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)243°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity 1.0E+14 - 1.0E+16ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 4.0hr
Dew Point -17.8°C
Processing (Melt) Temp 277 - 299°C
Mold Temperature 65.6 - 107°C
Injection Pressure 68.9 - 124MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
RTP 2700 S-70A Z RTP Company SEBS RTP
Spartech Polycom PP5230 Spartech Polycom PP Homopolymer Spartech
HANWHA KH-10 Hanwha Chemical PVC, Unspecified HANWHA
PETILEN YY S 0452 PETKIM Petrokimya Holding A.S. HDPE PETILEN
Sylvin 8369-80UV Grey 9589 Sylvin Technologies Incorporated PVC, Unspecified Sylvin