| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | DOMO Engineering Plastics GmbH |
| Trademark: | DOMAMID® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | y4qRIK_DOMAMID-A1-510-V30-I1-N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyamide 6, 30% glass fiber reinforced, impact modified, natural |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.34 | g/cm³ | ISO 1183 |
| Melt Volume-Flow Rate (MVR) (275°C/5.0 kg) | 18.0 | cm³/10min | ISO 1133 |
| Molding Shrinkage 1 | ISO 294-4 | ||
| Across Flow : 23°C, 72 hr | 1.1 | % | |
| Flow : 23°C, 72 hr | 0.50 | % | |
| Ash Content (650°C) | 30 | % | ISO 3451 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 8700 | MPa | ISO 527-2/1A/1 |
| Tensile Stress | ISO 527-2/1A/5 | ||
| Yield | 150 | MPa | |
| Break | 150 | MPa | |
| Tensile Strain (Break) | 4.0 | % | ISO 527-2/1A/20 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -30°C | 16 | kJ/m² | |
| 23°C | 26 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179/1eU | ||
| -30°C | 120 | kJ/m² | |
| 23°C | 110 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature | 222 | °C | ISO 11357-3 |
| Note Message | |
|---|---|
| 1 . | 50%RH, between 16 to 72 hrs |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Rigid Cast RC-8004 FR | BJB Enterprises, Inc. | PUR, Unspecified | Rigid Cast |
| Spartech Polycom PP5321 | Spartech Polycom | PP Homopolymer | Spartech |
| Tufpet PBT G2810 | Mitsubishi Rayon America Inc. | PBT | Tufpet |
| Daelim Po1y® LL-04SH | DAELIM INDUSTRIAL CO., LTD. | LLDPE | Daelim Po1y® |
| EcoPaXX® Q170E | DSM Engineering Plastics | Nylon 410 | EcoPaXX® |