| Category: | ABS , Acrylonitrile Butadiene Styrene |
| Manufacturer: | Techno Polymer Co, Ltd. |
| Trademark: | EXCELLOY |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | xkIPdC_EXCELLOY-SXJ220.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
EXCELLOY SXJ220 is an Acrylonitrile Butadiene Styrene (ABS) product. It can be processed by injection molding and is available in Asia Pacific or North America. Characteristics include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| UL File Number |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.08 | g/cm³ | ISO 1183, ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 21 | g/10 min | ISO 1133 |
| Molding Shrinkage | 0.50 to 0.70 | % | ISO 294-4 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 103 | ASTM D785, ISO 2039-2 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | |||
| Yield | 47.1 | MPa | ASTM D638 |
| Yield | 47.0 | MPa | ISO 527-2 |
| Flexural Modulus | |||
| -- | 2450 | MPa | ASTM D790 |
| -- | 2050 | MPa | ISO 178 |
| Flexural Strength | |||
| -- | 76.5 | MPa | ASTM D790 |
| -- | 72.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 18 | kJ/m² | ISO 179 |
| Notched Izod Impact | 190 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load | |||
| 0.45 MPa, Unannealed | 89.0 | °C | ASTM D648 |
| 0.45 MPa, Unannealed | 78.0 | °C | ISO 75-2/B |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+11 | ohms | ASTM D257 |
| Comparative Tracking Index | 750 | V | JIS L1094 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (ALL) | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 to 90.0 | °C | |
| Drying Time | 2.0 to 5.0 | hr | |
| Rear Temperature | 190 to 260 | °C | |
| Middle Temperature | 190 to 260 | °C | |
| Front Temperature | 190 to 260 | °C | |
| Mold Temperature | 40.0 to 80.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Aaroprene® TFIPP 2020 | Aaron Industries Corp. | PP, Unspecified | Aaroprene® |
| Ferro PP TPP30AF11HB NATURAL | Ferro Corporation | PP Homopolymer | Ferro PP |
| Luran® 378P G7 | Styrolution | SAN | Luran® |
| Osterlene® PPC-20-2.0-A | Osterman & Company | PP Impact Copolymer | Osterlene® |
| TABOREN® PM 29 T 20-027 | SILON s.r.o. | PP, Unspecified | TABOREN® |