| Category: | PP Copolymer , Polypropylene Copolymer |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYfill |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | xeHIAI_POLYfill-PPC-GF7020-PD2-E15.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre-reinforced Chemically coupled |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.04 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 7.0 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 0.90 to 1.1 | % | |
| Flow | 0.40 to 0.60 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 50.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 10 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 3600 | MPa | ISO 178 |
| Flexural Stress | 80.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -20°C | 13 | kJ/m² | |
| 23°C | 21 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 160 | °C | ISO 75-2/B |
| Vicat Softening Temperature | 155 | °C | ISO 306/A50 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.60 mm) | HB | UL 94 | |
| Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TECHNO ABS F5450 | Techno Polymer Co, Ltd. | ABS | TECHNO ABS |
| Ferro PP LPP25BK51BK | Ferro Corporation | PP, Unspecified | Ferro PP |
| Halene L 92001S | Haldia Petrochemicals Ltd. | LLDPE | Halene L |
| Lutene® XL2700BK | LG Chem Ltd. | PE, Unspecified | Lutene® |
| PIVINEL™ S-33-TELE | HELLENIC CABLES S.A. | PVC, Unspecified | PIVINEL™ |