Sarlink® TPV 2655

Category: TPV , Thermoplastic Vulcanizate
Manufacturer: Teknor Apex Company
Trademark: Sarlink® TPV
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: xbk2gK_Sarlink-TPV-2655.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Sarlink®TPV 2655 is a thermoplastic vulcanized rubber (TPV) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding.

Typical application areas include:
  • engineering/industrial accessories
  • building applications
  • Hose
  • application of coating
General Information
Uses
  • Plug
  • Washer
  • Washer
  • Pipe fittings
  • Shock Absorbing Pad
  • Weather-resistant sealing strip
  • Expansion Joint
  • Assembled glass
Appearance
  • Opacity
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.940g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)2.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A, 5 sec)64ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (100% Strain)2.41MPaASTM D412
Tensile Strength (Break)4.14MPaASTM D412
Tensile Elongation (Break)310%ASTM D412
Tear Strength 17.2kN/mASTM D624
Compression Set ASTM D395
    23°C, 22 hr 19%ASTM D395
    70°C, 22 hr 36%ASTM D395
ThermalNominal ValueUnitTest Method
Brittleness Temperature 1> -60.0°CASTM D746
InjectionNominal ValueUnit
Rear Temperature 173 - 213°C
Middle Temperature 179 - 219°C
Front Temperature 184 - 224°C
Nozzle Temperature 190 - 230°C
Processing (Melt) Temp 190 - 230°C
Mold Temperature 35.0 - 60.0°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Fast
Back Pressure 0.172 - 0.862MPa
Screw Speed 50 - 120rpm
Cushion 3.81 - 25.4mm
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 166 - 204°C
Cylinder Zone 2 Temp. 171 - 210°C
Cylinder Zone 3 Temp. 177 - 216°C
Cylinder Zone 5 Temp. 182 - 221°C
Die Temperature 190 - 227°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Note Message
1 .No Break @ -76°F.
Resin Grade Manufacturer Category Trademark
tefanyl® VR VRGR 809 Mitsubishi Chemical Performance Polymers, Inc. PVC, Rigid tefanyl® VR
WELLAMID Nylon 6000 GVZ 45 HWCP CP-Polymer-Technik GmbH & Co. KG Nylon 6 WELLAMID Nylon
ASPUN™ 6834 The Dow Chemical Company LLDPE ASPUN™
Clyrell RC249R LyondellBasell Industries PP Random Copolymer Clyrell
PENTAMID A L10 H natural PENTAC Polymer GmbH Nylon 66 PENTAMID A