| Andur 9000-AP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 90 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers. |
| General Information | |
|---|---|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.05 | g/cm³ | ASTM D792 |
| Thermoset | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Thermoset Mix Viscosity | ASTM D2393 | ||
| 21°C | 54000 | cP | ASTM D2393 |
| 70°C | 900 | cP | ASTM D2393 |
| 100°C | 200 | cP | ASTM D2393 |
| Additional Information |
|---|
| NCO: 4.8 to 5.3%Specific Gravity, ASTM D792, 70°F: 1.05 g/mlSpecific Gravity, ASTM D792, 212°F: 1.04 g/ml |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Rilsamid® AESNO MED | Arkema | Nylon 12 | Rilsamid® |
| megol® CA 55 SV/P1 | API SpA | SEBS | megol® |
| GAPEX® RPP20EA10BK | Ferro Corporation | PP Homopolymer | GAPEX® |
| Grilamid® L 20 LF grey | EMS-GRIVORY | Nylon 12 | Grilamid® |
| Latilub 37 B01-02S | LATI S.p.A. | PLA | Latilub |