Category: | LDPE , Low Density Polyethylene |
Manufacturer: | Osterman & Company |
Trademark: | Osterlene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | wbDw9l_OsterleneLDC1821A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
|
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.921 | g/cm³ | ASTM D1505 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 1.8 | g/10 min | ASTM D1238 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
secant modulus | ASTM D882 | ||
1% secant, MD | 179 | MPa | ASTM D882 |
1% secant, TD | 207 | MPa | ASTM D882 |
Tensile Strength | ASTM D882 | ||
MD : Yield | 10.3 | MPa | ASTM D882 |
TD : Yield | 11.0 | MPa | ASTM D882 |
MD : Fracture | 27.6 | MPa | ASTM D882 |
TD : Fracture | 23.4 | MPa | ASTM D882 |
Tensile Elongation | ASTM D882 | ||
MD : Fracture | 300 | % | ASTM D882 |
TD : Fracture | 500 | % | ASTM D882 |
Dart Drop Impact 1 | 90 | g | ASTM D1709 |
Elmendorf Tear Strength | ASTM D1922 | ||
MD | 360 | g | ASTM D1922 |
TD | 200 | g | ASTM D1922 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 100 | °C | ASTM D1525 |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Gloss (45°) | 70 | ASTM D2457 | |
Haze | 5.0 | % | ASTM D1003 |
Note Message | |
---|---|
1 . | F50 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
NatureFlex™ NE White | Innovia Films Ltd. | Cellulose, Regenerated | NatureFlex™ |
AZDEL™ U421B02N (Longitudinal) | Azdel, Inc. | PP Alloy | AZDEL™ |
Grilon® TSG-50/4 FA | EMS-GRIVORY | Nylon 66/6 | Grilon® |
KPOL-PP K-PPR 26.0 | KPOL Chem Co. | PP Random Copolymer | KPOL-PP |
Medalist® MD-53288 (PRELIMINARY DATA) | Teknor Apex Company | TPE | Medalist™ |