| Category: | EPM , Ethylene Propylene Copolymer |
| Manufacturer: | Melos GmbH |
| Trademark: | Melos™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | wBMmFb_Melos-FM-958.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Migration stabilised bedding compound for PVC insulation and PVC sheathing. Bedding compound for cables and wire with max. 90°C operating temperature at conductor. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.95 | g/cm³ | ISO 1183/A |
| Mooney Viscosity (ML 1+4, 100°C) | 25 | MU | DIN 53523 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A) | 75 | ISO 7619 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | > 1.0E+9 | ohms | VDE 0472 |
| Volume Resistivity (27°C) | > 1.0E+12 | ohms·cm | VDE 0472 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 80.0 to 100 | °C | |
| Cylinder Zone 2 Temp. | 90.0 to 110 | °C | |
| Cylinder Zone 3 Temp. | 90.0 to 110 | °C | |
| Cylinder Zone 4 Temp. | 95.0 to 115 | °C | |
| Adapter Temperature | 95.0 to 115 | °C | |
| Head Temperature | 100 to 120 | °C | |
| Extruder Screw L/D Ratio | 12.0:1.0 to 25.0:1.0 | ||
| Extruder Screw Temperature | 60 to 80 | °C | |
| Die Temperature | 100 to 120 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PRL AH-GP3 | Polymer Resources Ltd. | Acetal (POM) Homopolymer | PRL |
| WELLAMID Nylon 6000 HWCP | CP-Polymer-Technik GmbH & Co. KG | Nylon 6 | WELLAMID Nylon |
| DESLON™ 6 DSC101M6 | DESCO Co., Ltd. | Nylon 6 | DESLON™ 6 |
| MAJORIS FW214 - 8229 | AD majoris | PP, Unspecified | MAJORIS |
| POLYFLON™ L-5F | DAIKIN AMERICA, INC. | PTFE | POLYFLON™ |