Telcar® TL-1522A

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Telcar®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: w8YPQA_Telcar-TL-1522A.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Telcar®TL-1522A is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding.

Typical application areas include:
  • Automotive Industry
  • engineering/industrial accessories
General Information
Uses
  • Blow molding applications
  • Washer
  • Weather-resistant sealing strip
  • Application in Automobile Field
  • Car interior parts
  • Automotive exterior parts
  • Car exterior decoration
  • General
Appearance
  • Opacity
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.05g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)69g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)40ASTM D2240
MechanicalNominal ValueUnitTest Method
Taber Abrasion Resistance ASTM D2228
    1000 Cycles, 1000g, H-18 wheel 950mgASTM D2228
    1000 Cycles, 1000g, H-22 wheel 950mgASTM D2228
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 2.07MPaASTM D412
    300% strain 3.65MPaASTM D412
Tensile Strength (Break)4.96MPaASTM D412
Tensile Elongation (Break)580%ASTM D412
Tear Strength 113.0kN/mASTM D1004
Compression Set ASTM D395
    23°C, 22 hr 24%ASTM D395
    70°C, 22 hr 64%ASTM D395
    100°C, 22 hr 95%ASTM D395
ElectricalNominal ValueUnitTest Method
Volume Resistivity ASTM D257
    23°C 7.2E+15ohms·cmASTM D257
    50°C 9.5E+18ohms·cmASTM D257
InjectionNominal ValueUnit
Rear Temperature 171 - 193°C
Middle Temperature 177 - 199°C
Front Temperature 182 - 204°C
Nozzle Temperature 188 - 210°C
Processing (Melt) Temp 188 - 210°C
Mold Temperature 25.0 - 65.6°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.345MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 166 - 188°C
Cylinder Zone 2 Temp. 171 - 193°C
Cylinder Zone 3 Temp. 177 - 199°C
Cylinder Zone 5 Temp. 182 - 204°C
Die Temperature 190 - 210°C
Extrusion instructions
螺杆转速30 - 100 rpm
Note Message
1 .C mould
Resin Grade Manufacturer Category Trademark
Vital-Line SHM1332 Teknor Apex Asia Pacific PTE. LTD. PVC, Rigid Vital-Line
BRALEN® FB 08-64 Slovnaft Petrochemicals, s.r.o. LDPE BRALEN®
Jamplast JPPCABS10 Jamplast, Inc. PC+ABS Jamplast
LUVOCOM® 1105-7907 VP Lehmann & Voss & Co. PEEK LUVOCOM®
Macromeric® 0110-108 BK Saco Polymers CPE Macromeric®