RTP 1387 L

Category: PPS , Polyphenylene Sulfide
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: w4gqdw_RTP-1387-L.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Carbon Fiber - Lubricated
General Information
Filler / Reinforcement
  • Carbon Fiber, 40% Filler by Weight
Additive
  • Lubricant
Features
  • Lubricated
RoHS Compliance
  • Contact Manufacturer
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.48g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.050%ASTM D955
Moisture Content 0.040%
Additional InformationNominal ValueUnit
Primary Additive 40%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 32400MPaASTM D638
Tensile Strength 193MPaASTM D638
Tensile Elongation (Yield)0.80%ASTM D638
Flexural Modulus 28300MPaASTM D790
Flexural Strength 269MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)53J/mASTM D256
Unnotched Izod Impact (3.20 mm)320J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)268°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity < 1.0E+5ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)V-0UL 94
InjectionNominal ValueUnit
Drying Temperature 149°C
Drying Time 6.0hr
Processing (Melt) Temp 307 to 329°C
Mold Temperature 135 to 177°C
Injection Pressure 68.9 to 103MPa
Resin Grade Manufacturer Category Trademark
MAZMID B 150 FV 35 Mazzaferro Indústria e Comércio de Polímeros e Fibras Ltda. Nylon 6 MAZMID B
Southland AES Resin Southland Polymers AES Southland
Fainplast PVC PHA 81 Fainplast Compounds S.r.l PVC, Flexible Fainplast PVC
Fainplast PVC GK 80 Fainplast Compounds S.r.l PVC, Unspecified Fainplast PVC
OTECH PVC OC6014-Sandal OTECH Corporation PVC, Unspecified OTECH PVC