Medalist® MD-555

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Medalist™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: w3fXbk_MedalistMD555.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Medalist MD-555 is a high performance thermoplastic elastomer intended for use in medical and healthcare applications, especially medical tubing. Medalist MD-555 is a medium hardness, low density, clear grade designed to be a sustainable alternative to flexible PVC with excellent processability and throughput in extruded tubing.
General Information
Features
  • Low Specific Gravity
  • High purity
  • Low density
  • Pressure cooker disinfection
  • Good disinfection
  • Ethylene oxide disinfection
  • Anti-gamma radiation
  • Workability, good
  • Good adhesion
  • Good chemical resistance
  • Definition, high
  • No kinetic components
  • Halogen-free
  • Medium hardness
Uses
  • Films
  • Pipe fittings
  • Rubber substitution
  • Drug
  • Medical/nursing supplies
RoHS Compliance
  • RoHS compliance
Appearance
  • Clear/transparent
Forms
  • Particle
Processing Method
  • Extrusion
  • cast film
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.888g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)15g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 1 sec 55ASTM D2240
    Shaw A, 5 seconds 53ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    50% strain 1.52MPaASTM D412
    100% strain 1.86MPaASTM D412
    300% strain 2.86MPaASTM D412
Tensile Strength (Break)9.20MPaASTM D412
Tensile Elongation (Break)890%ASTM D412
Tear Strength 31.0kN/mASTM D624
Compression Set (23°C, 22 hr)9.1%ASTM D395
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 127 - 149°C
Middle Temperature 138 - 160°C
Front Temperature 149 - 171°C
Nozzle Temperature 171 - 193°C
Processing (Melt) Temp 171 - 193°C
Mold Temperature 21 - 38°C
Injection Pressure 1.38 - 5.52MPa
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 171 - 188°C
Cylinder Zone 2 Temp. 182 - 196°C
Cylinder Zone 3 Temp. 185 - 204°C
Cylinder Zone 4 Temp. 185 - 204°C
Cylinder Zone 5 Temp. 204 - 227°C
Die Temperature 204 - 227°C
Extrusion instructions
Screw Speed: 30 to 100 rpm.Screen Pack Recommendation:60/200/200/60 to 60/200/400/400/200/60 mesh size.
Resin Grade Manufacturer Category Trademark
VINIKA® CB70KA Mitsubishi Chemical Performance Polymers, Inc. PVC, Flexible VINIKA®
KOPA® KN173HI4 Kolon Plastics, Inc. Nylon 6 KOPA®
LOFEX® A3111 Lotte Chemical Corporation PET LOFEX®
MAJORIS DT267 AD majoris PP, Unspecified MAJORIS
Petrothene® LT493721 LyondellBasell Industries HDPE Petrothene®