Category: | Nylon 12 , Polyamide 12 |
Manufacturer: | EMS-GRIVORY |
Trademark: | Grilamid® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | vyAAzL_Grilamid-LV-23H.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Grilamid® LV-23H is a Polyamide 12 (Nylon 12) material filled with 23% glass fiber. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for injection molding. Important attributes of Grilamid® LV-23H are:
Typical applications include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.17 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 0.70 | -- | % | |
Flow | 0.10 | -- | % | |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 1.2 | -- | % | |
Equilibrium, 23°C, 50% RH | 0.60 | -- | % |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Shore Hardness (Shore D, 15 sec) | -- | 75 | ISO 868 | |
Ball Indentation Hardness | -- | 110 | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 5800 | 5000 | MPa | ISO 527-2 |
Tensile Stress (Break) | 110 | 95.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 7.0 | 9.0 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | -- | 12 | kJ/m² | |
23°C | -- | 20 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | -- | 85 | kJ/m² | |
23°C | -- | 80 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
1.8 MPa, Unannealed | 155 | -- | °C | ISO 75-2/A |
8.0 MPa, Unannealed | 80.0 | -- | °C | ISO 75-2/C |
Continuous Use Temperature | Internal Method | |||
-- 1 | 90.0 to 120 | -- | °C | |
-- 2 | 150 | -- | °C | |
Melting Temperature 3 | 178 | -- | °C | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 2.0E-5 | -- | cm/cm/°C | |
Transverse | 1.5E-4 | -- | cm/cm/°C |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | -- | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | -- | 1.0E+13 | ohms·cm | IEC 60093 |
Electric Strength | -- | 35 | kV/mm | IEC 60243-1 |
Comparative Tracking Index | -- | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification (0.800 mm) | HB | -- | IEC 60695-11-10, -20 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Type | PA12, MH, 18-060, GF23 | -- | ISO 1874 |
Note Message | |
---|---|
1 . | Long Term |
2 . | Short Term |
3 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1203-80D | RTP Company | TPU-Polyester | RTP |
POLYTROPE® STR 1030EU-01 NATURAL | A. Schulman Inc. | Polyolefin, Enhanced TPO | POLYTROPE® |
TEREZ PA 6.6 7100 | TER HELL PLASTIC GMBH | Nylon 66 | TEREZ PA 6.6 |
KOPET® KP133G15GN | Kolon Plastics, Inc. | PET | KOPET® |
KOCETAL® KH702 | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |