Dynaprene® VE2164A is a Thermoplastic Elastomer (TPE) material. It is available in Asia Pacific for injection molding. Important attributes of Dynaprene® VE2164A are:
|
General Information | |
---|---|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.958 | g/cm³ | ASTM D792 |
Moisture Content | < 0.060 | % | Internal Method |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 65 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress - Across Flow (100% Strain) | 2.22 | MPa | ASTM D412 |
Tensile Strength - Across Flow (Yield) | 5.52 | MPa | ASTM D412 |
Tensile Elongation - Across Flow (Break) | 400 | % | ASTM D412 |
Tear Strength - Across Flow 1(23°C) | 31.5 | kN/m | ASTM D624 |
Compression Set (100°C, 22 hr) | 30 | % | ASTM D395B |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Volume (121°C, 24 hr, in IRM 903 Oil) | 78 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | < -51.1 | °C | ASTM D746 |
Note Message | |
---|---|
1 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 203 SI 2 | RTP Company | Nylon 66 | RTP |
Pro-fax SL254M | INDELPRO, S.A. de C.V. | PP Random Copolymer | Pro-fax |
Zenite® 7145L | Celanese Corporation | LCP | Zenite® |
Chemfluor FEP | Saint Gobain - Norton | FEP | Chemfluor |
OP - ABS ABS 40CCF | Oxford Polymers | ABS | OP - ABS |