Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Teknor Apex Company (Chem Polymer) |
Trademark: | Chemlon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | vseSL5_Chemlon-109.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Chemlon® 109 is a Polyamide 66 (Nylon 66) material. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Chemlon® 109 are:
Typical application of Chemlon® 109: Automotive |
General Information | |
---|---|
Features |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.09 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 1.9 to 2.5 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 51.7 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield | 4.5 | % | |
Break | 50 | % | |
Flexural Modulus | 1720 | MPa | ASTM D790 |
Flexural Strength | 48.3 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | ASTM D256 | ||
-40°C | 240 | J/m | |
23°C | 960 | J/m |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 62.8 | °C | ASTM D648 |
Melting Temperature | 257 | °C | DSC |
RTI Elec (0.749 mm) | 65.0 | °C | UL 746 |
RTI Imp (0.749 mm) | 65.0 | °C | UL 746 |
RTI Str (0.749 mm) | 65.0 | °C | UL 746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+13 | ohms·cm | ASTM D257 |
Dielectric Strength (3.00 mm) | 10 | kV/mm | ASTM D149 |
Comparative Tracking Index (CTI) | 600 | V | UL 746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.749 mm) | HB | UL 94 | |
Oxygen Index | 21 | % | ASTM D2863 |
FMVSS Flammability | PASSES | FMVSS 302 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Suggested Max Moisture | 0.20 | % | |
Suggested Max Regrind | 25 | % | |
Rear Temperature | 241 to 257 | °C | |
Middle Temperature | 257 to 271 | °C | |
Front Temperature | 263 to 279 | °C | |
Nozzle Temperature | 263 to 282 | °C | |
Processing (Melt) Temp | 263 to 282 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TAROPRENE® 1 A85 E1N | Taro Plast S.p.A. | TPV | TAROPRENE® |
TES J-50/20/RG | Techmer Engineered Solutions | PC | TES |
Hifax HSBM CB 1158 A | LyondellBasell Industries | PP Impact Copolymer | Hifax |
DURACON® LW-02 | Polyplastics Co., Ltd. | Acetal (POM) Copolymer | DURACON® |
Osterlene® GPPS0900 | Osterman & Company | PS (GPPS) | Osterlene® |