Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | Franplast S.r.l. |
Trademark: | Franprene |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | veU1du_Franprene-TVA-9155.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
SEBS based compound ideal for the manufacturing of extruded products, such as window rubber strips, gaskets etc. Injection processing is possible too. Endowed with good elastic properties and resistant to external agents. Application:
|
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.940 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 25 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A) | 55 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Break) | 10.0 | MPa | ISO 527-2 |
Nominal Tensile Strain at Break | 1000 | % | ISO 527-2 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength | 30 | kN/m | ISO 34-1 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -30 to 90 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Time | 0.0 | hr | |
Cylinder Zone 1 Temp. | 110 to 140 | °C | |
Cylinder Zone 2 Temp. | 125 to 155 | °C | |
Cylinder Zone 3 Temp. | 145 to 175 | °C | |
Cylinder Zone 4 Temp. | 150 to 180 | °C | |
Die Temperature | 115 to 165 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Razalen® P121 GR20 | Razin™ Engineering Plastics | PP Impact Copolymer | Razalen® |
Yuyao PBT 3055G20 | Yuyao Tenglong Plastics Co., Ltd. | PBT | Yuyao PBT |
ISPLEN® PP 084 D2M | REPSOL | PP Homopolymer | ISPLEN® |
KANEKA H527 | Kaneka North America LLC | CPVC | KANEKA |
TORZEN® HV240A NC01 | INVISTA Engineering Polymers | Nylon 66 | TORZEN® |