Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Wellman Engineering Resins |
Trademark: | Wellamid® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | vBL2Yg_Wellamid-MRGF25-15-42H-N2-WE1705-N2.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Wellamid® MRGF25/15 42H-N2/WE1705-N2 is a Polyamide 6 (Nylon 6) material filled with 40% glass\mineral. It is available in Asia Pacific, Europe, Latin America, or North America. Primary attribute of Wellamid® MRGF25/15 42H-N2/WE1705-N2: Good Aesthetics. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.49 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow : 23°C | 0.60 to 1.0 | % | |
Flow : 23°C | 0.20 to 0.60 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 135 | MPa | ISO 527-2 |
Tensile Strain (Yield, 23°C) | 2.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 9800 | MPa | ISO 178 |
Flexural Stress (23°C) | 190 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C) | 5.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 200 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 220 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sumitomo PE B2555 | Sumitomo Chemical Asia | HDPE | Sumitomo PE |
ACCUTECH™ HP0336G20CL | ACLO Compounders Inc. | PP Homopolymer | ACCUTECH™ |
ExxonMobil™ LDPE LD 150 Series | ExxonMobil Chemical | LDPE | ExxonMobil™ LDPE |
KOCETAL® WR701LO | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
Ixef® 3008 | Solvay Specialty Polymers | PARA | Ixef® |