FRAGOM PR/721

Category: Polyolefin, Unspecified , Polyolefin
Manufacturer: Crosspolimeri S.p.A.
Trademark: FRAGOM
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: uvGmmu_FRAGOM-PR-721.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
FRAGOM PR PR/720 is the trade-mark of our flame retardant polyolefinic compounds.
FRAGOM PR PR/720 is a halogen-free flame-retardant polyolefinic thermoplastic compound with high values of temperature index and oxygen index, very easy to process
and suitable for cable sheathing.

The compound was developed to use in sheathing extrusion expecially when the thikness is important (1,8-2,4 mm)

Certify: CEI 2011 M1,VDE 0207 HM2,BS 7655 LTS1-LTS3
General Information
Features
  • Workability, good
  • Halogen-free
  • Flame retardancy
Uses
  • Cable sheath
  • Wire and cable applications
Agency Ratings
  • BS 7655 LTS 1-3
  • CEI 2011 M1
  • VDE 0207 HM2
Forms
  • Particle
Processing Method
  • Extrusion
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.51g/cm³ASTM D792
Melt Mass-Flow Rate (MFR)
    190°C/21.6 kg 20g/10 minASTM D1238
    280°C/0.325 kg 6.0g/10 minIEC 60811
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)46ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Stress (Yield)> 13.0MPaIEC 60811
Tensile Strain (Break)190%IEC 60811
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air (100°C, 168 hr)5.0%IEC 60811
Change in Tensile Strain at Break in Air (100°C, 168 hr)-14%IEC 60811
Change in Tensile Strength (70°C, 4 hr, in SAE 20 Oil)< 15%IEC 60811
Change in Tensile Strain at Break (70°C, 4 hr, in SAE 20 Oil)< 10%IEC 60811
ThermalNominal ValueUnitTest Method
Hot Pressure Test - Penetration 1(80°C)%IEC 60811
FlammabilityNominal ValueUnitTest Method
Halogen Content %IEC 60754-1
Oxygen Index 40%ASTM D2863
Additional Information
No detrimental effects on properties and capability of FRAGOM in presence of Masterbatch colours, black included.We suggest to dry masterbatch before using.
ExtrusionNominal ValueUnit
Drying Temperature 80.0 - 90.0°C
Drying Time 2.0 - 3.0hr
Cylinder Zone 1 Temp. 120°C
Cylinder Zone 2 Temp. 135°C
Cylinder Zone 3 Temp. 150°C
Cylinder Zone 4 Temp. 160°C
Cylinder Zone 5 Temp. 165°C
Die Temperature 175°C
Note Message
1 .K=0.6, 4 hr
Resin Grade Manufacturer Category Trademark
PRIMALLOY® B1700 Mitsubishi Chemical Performance Polymers, Inc. TPE PRIMALLOY®
GPPC ABS D-1000A GPPC Chemical Co., Ltd. ABS GPPC ABS
Eltex® P CAP912 INEOS Olefins & Polymers Europe PP Random Copolymer Eltex® P
EL-Lene™ H5211PBL SCG Chemicals Co., Ltd. HDPE EL-Lene™
HiFill® MD PA66 0125 LE Techmer Engineered Solutions Nylon 66 HiFill®