Mecoline S TP 1006 F

Category: TP, Unspecified , Thermoplastic
Manufacturer: Melos GmbH
Trademark: Mecoline
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: uG87bO_Mecoline-S-TP-1006-F.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Halogen-free, low smoke, thermoplastic, highly flame retardant compound for the sheathing of low and medium voltage cables in General Installation applications.
General Information
Additive
  • Flame Retardant
Features
  • Flame Retardant
  • Halogen Free
  • Low Smoke Emission
Uses
  • Cable Jacketing
  • Low Voltage Insulation
  • Medium Voltage Insulation
  • Wire & Cable Applications
Agency Ratings
  • BS 6724
  • BS 7655:6.1 Type LTS 2
  • CEI 2011 M1
  • EN 50363-8 TM7
  • IEC 60092-359 SHF-1
  • NFC 32-323
  • VDE 0207 part 24 HM2
  • VDE 0207 part 24 HM4
  • VDE 0250 part 215 HM5
  • VDE 0276 part 604 HM4
  • VDE 0281 part 14 TM7
RoHS Compliance
  • RoHS Compliant
Forms
  • Pellets
Processing Method
  • Extrusion
PhysicalNominal ValueUnitTest Method
Density 1.56g/cm³ISO 1183/A
Melt Mass-Flow Rate (MFR) (160°C/21.6 kg)5.0g/10 minISO 1133
pH > 4.5DIN VDE 0472
ThermalNominal ValueUnitTest Method
Hot Pressure Test - penetration 6h at 90°C 27%DIN VDE 0472
Temperature Index 280°CASTM D2863
ElectricalNominal ValueUnitTest Method
Conductivity < 10.0µS/mm
ExtrusionNominal ValueUnit
Head Temperature 140 to 160°C
Extruder Screw L/D Ratio 20.0:1.0 to 25.0:1.0
Extruder Screw Compression Ratio 1.0:1.2
HardnessNominal ValueUnitTest Method
Shore Hardness (Shore D)50ISO 7619
MechanicalNominal ValueUnitTest Method
Tensile Stress 10.3MPaIEC 811-1-1
Tensile Strain (Break)180%IEC 811-1-1
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air IEC 811-1-2
    100°C, 240 hr -9.7%
    120°C, 168 hr 1.9%
Change in Tensile Strain at Break in Air IEC 811-1-2
    100°C, 240 hr 11%
    120°C, 168 hr 11%
ThermalNominal ValueUnitTest Method
Brittleness Temperature -20.0°CASTM D746
ElectricalNominal ValueUnitTest Method
Surface Resistivity 1> 1.0E+12ohmsDIN VDE 0303
Volume Resistivity 2> 1.0E+12ohms·cmDIN VDE 0303
FlammabilityNominal ValueUnitTest Method
Oxygen Index 45%ASTM D2863
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 110 to 130°C
Cylinder Zone 2 Temp. 115 to 135°C
Cylinder Zone 3 Temp. 120 to 140°C
Cylinder Zone 4 Temp. 125 to 145°C
Cylinder Zone 5 Temp. 130 to 150°C
Adapter Temperature 135 to 155°C
Die Temperature 150 to 170°C
Note Message
1 .16h at 20°C, 500V
2 .16h at 20°C, 500V
Resin Grade Manufacturer Category Trademark
PRL PC-UV4 Polymer Resources Ltd. PC PRL
RAMCLEAN™ 101 Polyram Ram-On Industries TP, Unspecified RAMCLEAN™
SLOVAMID® 6 GB 30 TS Plastcom Nylon 6 SLOVAMID® 6
DuraStar™ MN610 Eastman Chemical Company Polyester, TP DuraStar™
Eltex® Superstress™ CAP602S2 INEOS Olefins & Polymers Europe HDPE Copolymer Eltex®