RTP 4007 A

Category: PPA , Polyphthalamide
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: uFyUOX_RTP-4007-A.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 40% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.52g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.40%ASTM D955
Water Absorption (23°C, 24 hr)0.20%ASTM D570
Moisture Content 0.10%
Additional InformationNominal ValueUnit
Primary Additive 40%
HardnessNominal ValueUnitTest Method
Rockwell Hardness (R-Scale)125ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Modulus 12400MPaASTM D638
Tensile Strength 207MPaASTM D638
Tensile Elongation (Yield)2.0%ASTM D638
Flexural Modulus 13100MPaASTM D790
Flexural Strength 303MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)91J/mASTM D256
Unnotched Izod Impact (3.20 mm)640J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)277°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity > 1.0E+15ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 107°C
Drying Time 4.0 - 6.0hr
Dew Point -28.9°C
Processing (Melt) Temp 329 - 343°C
Mold Temperature 65.6 - 163°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
Braskem PP HP 525M Braskem PP Homopolymer Braskem PP
Axiall PVC 22871 Axiall Corporation PVC, Flexible Axiall PVC
LEXAN™ 133R resin SABIC Innovative Plastics Asia Pacific PC LEXAN™
Dryflex® SE 60A301N U ELASTO SEBS Dryflex®
SCHULABLEND® (ABS/PA) M/MK 6501 U A. Schulman Europe ABS+Nylon SCHULABLEND®