Category: | PS (HIPS) , High Impact Polystyrene |
Manufacturer: | PolyOne Corporation |
Trademark: | Edgetek™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | uAx1Dw_Edgetek-ET7400-5005-WHITE-VN-3926.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Edgetek™ET7400-5005 WHITE VN 3926 is a high impact polystyrene product,. It is available in Europe or Europe. Typical application areas are: electrical/electronic applications. |
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density 1 | 1.13 | g/cm³ | ISO 1183 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 3300 | MPa | ISO 527-2/1 |
Tensile Stress (Yield, 23°C) | 28.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 3.5 | % | ISO 527-2 |
Flexural Modulus (23°C) | 3000 | MPa | ISO 178 |
Flexural Stress (23°C) | 44.0 | MPa | ISO 178 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 105 | °C | ISO 306/A50 |
Additional Information |
---|
The product needs to be pre-dried before processing. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 60.0 | °C | |
Drying Time - Desiccant Dryer | 4.0 | hr | |
Processing (Melt) Temp | 210 - 230 | °C |
Note Message | |
---|---|
1 . | ±0.03 g/cm³ |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Colorite 11 Series 6811 | Colorite Polymers | PVC, Unspecified | Colorite 11 Series |
FHR EPS 71-7371 | Flint Hills Resources, LP | PS (EPS) | FHR EPS |
Elastollan® R 1001 | BASF Polyurethanes GmbH | TPU-Polyester | Elastollan® |
Karina IVORY PVC COMPOUND 105800-35/1-B-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
SQUARE® SSR1503-40 | Shenzhen SQUARE Silicone Co., Ltd. | Silicone | SQUARE® |