Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Radici Plastics |
Trademark: | Radilon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | uAKLbU_Radilon-S-BF-990-GRI.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
PA6 injection moulding grade. Low friction. Natural grey colour. Suitable for parts and components requiring low friction and improved wear resistance, such as gears, bearings, and cams. ISO 1043 : PA6 |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Appearance |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.14 | -- | g/cm³ | ISO 1183 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 3200 | -- | MPa | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 75.0 | -- | MPa | ISO 527-2/1A/50 |
Tensile Strain (Yield) | 3.5 | -- | % | ISO 527-2/1A/50 |
Nominal Tensile Strain at Break | 20 | -- | % | ISO 527-2/1A/50 |
Flexural Modulus 1 | 2700 | -- | MPa | ISO 178 |
Flexural Stress 2 | 100 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 4.0 | -- | kJ/m² | |
23°C | 5.5 | -- | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 70.0 | -- | °C | ISO 75-2/Af |
Vicat Softening Temperature | 200 | -- | °C | ISO 306/B50 |
Melting Temperature 3 | 220 | -- | °C | ISO 11357 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+12 | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Rate | 0.0 | -- | mm/min | FMVSS 302 |
Flame Rating (0.800 mm) | HB | -- | UL 94 | |
Glow Wire Flammability Index (2.00 mm) | 650 | -- | °C | IEC 60695-2-12 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 80.0 | °C | |
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr | |
Dew Point - Desiccant Dryer | < -20.0 | °C | |
Suggested Max Moisture | 0.15 | % | |
Processing (Melt) Temp | 250 to 280 | °C | |
Mold Temperature | 70.0 to 80.0 | °C | |
Injection Rate | Moderate |
Note Message | |
---|---|
1 . | 2.0 mm/min |
2 . | 2.0 mm/min |
3 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Retpol® PDR 1619/4 HS | PolyPacific Pty. Ltd. | PP Homopolymer | Retpol® |
CERTENE™ PHM-5A | Muehlstein | PP Homopolymer | CERTENE™ |
Hydrin® C2000LL | Zeon Chemicals L.P. | Epoxy | Hydrin® |
Magnobond 91 | Magnolia Plastics, Inc. | Epoxy | Magnobond |
Mafill® CR CE 5044 | Ravago Group | PP Copolymer | Mafill® |