Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Bada AG |
Trademark: | Badamid® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | u7iXnA_Badamid-LB70-GF-M35-FR-HF.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Halogen free flame retardant, 35% glass fibres and mineral reinforced injection moulding grade with superior mechanical properties |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.37 | -- | g/cm³ | ISO 1183 |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 5.7 to 6.3 | -- | % | |
Equilibrium, 23°C, 50% RH | 1.7 to 2.1 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus 1(23°C) | 8000 | 3800 | MPa | ISO 527-2/1 |
Tensile Stress 2(Break, 23°C) | 90.0 | 50.0 | MPa | ISO 527-2/5 |
Tensile Strain 3(Break, 23°C) | 2.5 | 6.0 | % | ISO 527-2/5 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 3.8 | 5.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 45 | 100 | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 210 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 170 | -- | °C | ISO 75-2/A |
Melting Temperature (DSC) 4 | 222 | -- | °C | ISO 3146 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+13 | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+13 | 1.0E+10 | ohms·cm | IEC 60093 |
Relative Permittivity (1 MHz) | 3.50 | 5.50 | IEC 60250 | |
Dissipation Factor (1 MHz) | 0.014 | 0.16 | IEC 60250 | |
Comparative Tracking Index | 550 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating | UL 94 | |||
0.800 mm | V-2 | -- | ||
1.60 mm | V-2 | -- |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 to 4.0 | hr | |
Processing (Melt) Temp | 250 to 270 | °C | |
Mold Temperature | 60.0 to 90.0 | °C |
Note Message | |
---|---|
1 . | Test Specimen accordng to ISO 3167, Type A |
2 . | Test Specimen accordng to ISO 3167, Type A |
3 . | Test Specimen accordng to ISO 3167, Type A |
4 . | 10 K/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 2099 X 134514 | RTP Company | PLA | RTP |
DOMAMID® 6G25V0EF | DOMO Engineering Plastics SPA | Nylon 6 | DOMAMID® |
Eastobond™ 19412 | Eastman Chemical Company | Copolyester | Eastobond™ |
EMLON® 66 GFR 15 | EMAS Plastik San.Tic.AS. | Nylon 66 | EMLON® |
TechnoElast A 8000 I 1 nat | TechnoCompound GmbH | TPE | TechnoElast |