Andur 8500 AP/Curene® 442

Category: PUR-Ether/TDI , Polyurethane (Polyether, TDI)
Manufacturer: Anderson Development Company
Trademark: Andur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: tyZhPx_Andur-8500-AP-Curene-442.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Andur 8500-AP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 85 to 87 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.12g/cm³ASTM D1505
Molding Shrinkage - Flow 1.3%ASTM D955
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)86ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 6.21MPaASTM D412
    300% strain 15.2MPaASTM D412
Tensile Strength (Yield)23.4MPaASTM D412
Tensile Elongation (Break)400%ASTM D412
Compression Set 30%ASTM D395B
Bayshore Resilience 30%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 7.0 - 8.0min
Demold Time (100°C)25min
Post Cure Time (100°C)4.0hr
Additional Information
Durometer Hardness, ASTM D2240, Shore A: 85 to 87Die C Tear, ASTM D1004: 350 pliAverage Split Tear, ASTM D1938: 82 pliStoichiometry Curative Level: 95%Cure Time, 150 to 160°F: OvernightMix Temperature: Andur 8500 AP: 160-212°F Curene 442: 250°F
Resin Grade Manufacturer Category Trademark
Premi-Glas® 1200H-10 Premix, Inc. TS, Unspecified Premi-Glas®
Ultramid® 8231G HS BK-102 BASF Corporation Nylon 6 Ultramid®
HONES® PBT GF10 Guangdong Shunde Hones Polymer Material Co., Ltd. PBT HONES®
Plenco 07507 (Transfer) Plastics Engineering Co. Phenolic Plenco
Maxxam™ H6 GF/30 H Black PolyOne Corporation PP Homopolymer Maxxam™